김규용, 구경모, 남정수, 신경수, & 이태규. (2012). 슬래그 결합재 모르타르의 압축강도 발현 성상. 대한건축학회 논문집-구조계, 28(9), 99-106.
김규용, 구경모, 남정수, 신경수, & 이태규. (2012). 슬래그 결합재 모르타르의 압축강도 발현 성상. 대한건축학회 논문집-구조계, 28(9), 99-106.
작성자 관리자
조회수 147 등록일 2012.09.01
주저자 김규용
교신저자 042-821-7731
공동저자 미야우치 히로유키, 구경모, 남정수, 이태규
학술지명 대한건축학회

Abstract
Recently, with the emphasis on green development, international efforts to lessen environmental problem is gaining momentum.
In order to achieve true green development, the primary task is to minimize environmental load such as energy and the CO2 emission levels due to the consumption of resources. As an effort to decrease CO2 emission levels, construction sites is lowering the use of cement and instead is actively promoting the use of industrial by-products such as blast-furnace slag cement and fly ash cement. As a part of this low-carbon green movement, the concrete industry is also largely replacing its general concrete with fly ash and blast-furnace slag concretes and between these two alternatives, the blast-furnace slag concrete is more widely used. The advantages of blast-furnace slag concrete may include lower hydration heating velocity, restraint on concrete temperature increase, long-age strength improvement due to latent hydraulic reaction, improved water tightness, and repulsion to chemical erosion. These advantages contribute to the high quality of the blast-furnace slag concrete.